Common abnormalities and treatment of injection molded produ
欄目:Industry News 發(fā)布時(shí)間:2021-06-03 15:19
Anomalous phenomenon, product, cause, solution Crack 1. The mold is too cold to adjust the mold temperature 2. Cooling time is too long, reducing cooling time 3. Plastic and metal inserts shrink differently. Metal inserts are preheated. 4....


Anomalous phenomenon, product, cause, solution
Crack 1. The mold is too cold to adjust the mold temperature
2. Cooling time is too long, reducing cooling time
3. Plastic and metal inserts shrink differently. Metal inserts are preheated.
4. The ejector device is unbalanced in inclination, and the ejector cross-sectional area is small or improperly distributed. Adjust the ejector device or reasonably arrange the number of ejector pins and their positions.
5. The production slope is not enough, the demoulding is difficult, and the draft angle is correctly designed.
There are ripples on the surface of the product. 1. The material temperature is low and the temperature is high.
2. Injection pressure The material temperature is high, which can reduce the injection pressure, and vice versa.
3. Low mold temperature Increase mold temperature or increase injection pressure
4. The injection speed is too slow. Increase the injection speed.
5. The gate is too small.
The brittleness of the product decreases. 1. The material temperature is too high, the plastic decomposes, the material temperature is lowered, and the residence time of the material in the barrel is controlled.
2. Excessive stress in plastics and inserts Preheat the inserts to ensure a certain thickness of plastic around the inserts
3. The number of times of plastic recycling is controlled.
4. Plastic water content, preheating and drying of raw materials
Difficulty in demoulding 1. Poor structure of the mold ejection device Improved ejection design
2. The mold cavity is not enough to correct the mold.
3. The cavity temperature is not suitable. The mold temperature is properly controlled.
4. The cavity has seams or materials. Clean the mold
5. The molding cycle is too short or too long. Properly control the injection cycle.
6. The core has no air inlet. Modify the mold.
Insufficient product size 1. Unstable machine circuit or oil system Corrected electrical or hydraulic system
2. The molding cycle is different. Control the molding cycle to make it consistent.
3. Temperature. time. Pressure change adjustment, control is basically the same
4. Plastic pellets vary in size. Use uniform plastic.
5. Uneven mixing ratio of recycled scrap and new material. Control mixing ratio to make uniform
6. Uneven feeding control or adjust the feeding evenly
Peeling and delamination of parts 1. Different plastics mixed with a single variety of plastic
2. Different grades of the same plastic are mixed with the same grade of plastic
3. Poor plasticization, increase molding temperature
4. Mix in foreign matter, clean up raw materials, and remove impurities.
Weld marks 1. The plastic temperature is too low. Increase the barrel. Nozzle and mold temperature
2. Too many gates Reduce the gate or change the gate location
3. Excessive release agent The atomization release agent is used. Reduce usage
4. The injection speed is too slow. Increase the injection speed.
5. The mold temperature is too low to increase the mold temperature
6. The injection pressure is too small to increase the injection pressure
7. Die exhaust is bad. Increase the mold vent hole.
Insufficient injection 1. Lower barrel and nozzle temperature Increase barrel and nozzle temperature
2. The mold temperature is low, and the mold temperature is raised.
3. Insufficient amount of feed, increase the amount of feed properly
4. The number of parts exceeds the maximum injection volume of the injection molding machine.
5. The runner and gate are too small. Increase the gate size appropriately.
6. The injection pressure is too low or the injection speed is too slow. Increase the injection pressure or increase the temperature, and increase the injection speed.

Wuxi Jiahong Plastic Technology Co., Ltd. has nearly 30 years of experience in research and development and granulation of modified PVC pellets. The professional technical service team can provide one-stop system solutions for customers. For more information about the product, please visit our official website: zhushibao.net, consult online customer service or call the hotline. Fixed line: 0510-68755207 Mobile: 15190220696, we will be happy to help you.

(Disclaimer: All the tutorials and resources included in this site are from the Internet, and the copyrights are owned by the original author and its website. Although this site strives to preserve the original copyright information, it may not be able to determine its origin due to various reasons. The true source, please forgive the original author! If you have any objection to the attribution of the tutorial and resources of this site, please notify Xiaobian immediately, the situation is true, we will delete it in the first time.)
久久久久亚洲AV无码专区首| 全部免费毛片在线播放| 久久久国产精华液| JAPAN少妇洗澡VIDEOS| 人人妻人人澡人人爽人人DVD| 亚洲AV日韩AV无码| JAPAN少妇洗澡VIDEOS| 午夜亚洲2020理论网站| 亚洲国产婷婷香蕉久久久久久| 人妻少妇无码精品视频区 | 亚洲欧美专区精品久| 日本在线电影一区二区三区| 色妺妺在线视频| 女公务员人妻呻吟求饶| 欧美超级乱婬视频播放| 国产人A片777777久久| 人妻丰满精品一区二区A片| 少妇愉情理伦片丰满丰满午夜| 国产欧美久久久精品免费| 久久精品欧美一区二∴今9| 中文字幕在线亚洲一区二区三区| 国产一区二区不卡在线播放| 99久久99久久免费精品小说| 国产精品99久久久久久猫咪| 亚洲国产成人综合一区二区三区| 欧美成人性生活在线视频| 啊轻点灬太粗嗯太深了用力 | 精品日本亚洲一区二区三区| A级国产乱理论片在线观看| 熟女性饥渴一区二区三区| 亚洲午夜久久久久久久69| 亚洲色偷偷AV男人的天堂| 很黄很黄吸奶头视频| 人人妻人人澡人人爽精品日本| 一级欧美一级日韩视频| 无人视频在线观看完整版高清| JIZZJIZZ少妇亚洲水多| 少妇高潮惨叫久久久久久| 久久精品日韩欧美久久| 亚洲精品人妻在线视频| 成年片人免费红杏直播|